Technical Operations & Maintenance Guide

Maintenance & Plate
Replacement Protocol

Precision backwash parameters, chemical cleaning formulations, zero-damage scraper calibration and a field fault-diagnosis checklist -- engineered to help mining maintenance teams extend ceramic filter plate service life to 13+ months while sustaining minimum cake moisture.

Plate Lifespan
13+ Months
Backwash Pressure
0.20 MPa
Flatness Tolerance
±0.3 mm
pH Resistance
1 - 14

SOP 01 -- Permeability Restoration

Scientific Backwash Standard Operating Procedure

Our integral water-casting and whole-body sintering process produces a monolithic alumina ceramic structure with no adhesive bond lines -- enabling safe operation at backwash pressures of 0.15-0.20 MPa, significantly above the ≤0.15 MPa ceiling of conventional bonded-segment plates. This higher pressure window is the key to flushing sub-micron mineral fines that low-pressure cycles leave embedded in pore channels.

Structural Advantage

Why monolithic sintering enables higher backwash pressure

Conventional ceramic filter plates are assembled from individual sectors bonded with adhesive or epoxy. Under repeated backwash cycles, these bond lines fatigue and delaminate -- limiting safe operating pressure to below 0.15 MPa. Our plates are formed and sintered as a single monolithic body: there are no bond interfaces to fail, no adhesive to swell or dissolve, and no delamination risk across the full pH 1-14 operating range.

Conventional bonded plate

< 0.15 MPa

Maximum safe backwash pressure

Our monolithic plate

0.15-0.20 MPa

Rated working backwash pressure

Integral sintered body -- zero bond lines

No adhesive interfaces across the full plate cross-section

Pulse backwash cycle -- field procedure

Execute the following sequence at each scheduled backwash interval. Do not substitute continuous-flow backwash for pulse cycles -- the pressure surge of each pulse is what dislodges embedded mineral fines from the pore throat.

  1. Confirm system pressure before initiating

    Verify backwash water supply pressure at the manifold inlet. Target range: 0.15-0.20 MPa. Below 0.15 MPa, fine mineral particles will not be fully expelled from pore channels. Above 0.22 MPa, risk of micro-crack initiation increases -- install a pressure-relief valve if your supply line fluctuates.

    Critical parameter: 0.15-0.20 MPa
  2. Execute water pulse sequence

    Open the backwash valve for 3-5 seconds per sector, then close fully for 2 seconds before the next pulse. This on/off cycle creates a hydraulic hammer effect that mobilises compacted fines. Run a minimum of 3 consecutive pulses per sector per backwash session.

  3. Follow with compressed air purge

    Immediately after the water pulse sequence, apply a 0.10-0.15 MPa compressed air purge for 2-3 seconds per sector. The air displaces residual water and suspended fines from the pore network, preventing re-deposition as the plate re-enters the slurry tank. Combined water-air pulsing reduces pore blockage rate by up to 60% versus water-only backwash.

  4. Verify discharge water clarity

    Collect a sample of backwash discharge water after the final pulse. Water should clear from turbid to near-transparent within the 3-pulse sequence. Persistent turbidity after 5+ pulses indicates deep pore blockage requiring chemical cleaning -- do not continue routine backwash; escalate to the acid-wash protocol.

  5. Log and trend backwash performance

    Record the number of pulses required to achieve discharge clarity after each session. A rising trend -- more pulses needed over successive sessions -- is an early indicator of scale accumulation or pore narrowing. Use this data to trigger chemical cleaning before performance degradation becomes measurable in cake moisture.

SOP 02 -- Micropore Regeneration

Chemical Cleaning & Micropore Regeneration Guide

Backwash removes loose surface deposits. Scale -- calcium carbonate, iron hydroxide and silicate precipitates -- requires chemical dissolution. Our integral-sintered alumina ceramic is inert across pH 1-14 with no adhesive binders that could swell, dissolve or delaminate during prolonged acid immersion, enabling aggressive cleaning cycles that bonded plates cannot safely tolerate.

Iron Ore Applications

Iron Hydroxide & Carbonate Scale

Iron ore slurries produce ferric hydroxide (Fe(OH)₃) and siderite (FeCO₃) deposits that progressively narrow pore throats. These deposits respond well to oxalic acid, which forms soluble iron-oxalate complexes that are easily rinsed away.

Option A -- Oxalic Acid Wash (Recommended)

Concentration
3-5% w/v oxalic acid solution
Solution pH
1.5-2.5
Temperature
40-60 °C (accelerates dissolution)
Immersion time
60-120 min
Rinse protocol
3× clean water flush, verify pH > 6

Option B -- Citric Acid Wash (Milder Alternative)

Concentration
5-8% w/v citric acid solution
Solution pH
2.0-3.0
Immersion time
90-180 min
Best for
Light-to-moderate scale buildup

Copper Ore Applications

Calcium Sulphate & Silicate Scale

Copper flotation circuits commonly produce calcium sulphate (gypsum) and aluminosilicate scale from reagent residues. Gypsum is poorly soluble in weak acids -- dilute nitric acid or hydrochloric acid provides the ionic strength needed for effective dissolution.

Option A -- Dilute Nitric Acid Wash

Concentration
2-4% v/v dilute HNO₃
Solution pH
1.0-2.0
Temperature
Ambient (20-30 °C)
Immersion time
45-90 min
Rinse protocol
4× clean water flush, verify pH > 6

⚠ Use only in well-ventilated areas. Do not exceed 5% HNO₃ -- higher concentrations attack the alumina matrix at extended contact times.

Option B -- Hydrochloric Acid Wash

Concentration
3-5% v/v dilute HCl
Solution pH
1.0-1.5
Immersion time
30-60 min
Max safe concentration
10% HCl (do not exceed)

Why our plates withstand prolonged acid immersion without delamination

Conventional bonded-segment ceramic plates use organic adhesives or epoxy resins to join individual sectors. These binders are vulnerable to acid hydrolysis -- even dilute acid at pH 2 will progressively degrade bond strength over repeated cleaning cycles, leading to plate splitting and membrane delamination. Our integral-sintered monolithic structure contains no organic binders anywhere in the plate body. The alumina ceramic matrix is chemically inert from pH 1 to pH 14, allowing extended immersion cleaning (up to 4 hours) without any risk of structural separation. This means more thorough cleaning, more cleaning cycles per plate life, and a direct contribution to achieving 13+ months of service life.

Recommended chemical cleaning intervals by scale severity
Cleaning Level Method Trigger Condition Frequency Duration
Routine Backwash Water + air pulse Every shift, regardless of condition Every 8 hrs 3-5 min/disc
Light Acid Wash Citric acid 5-8% Backwash discharge still turbid after 5 pulses Weekly 90-180 min soak
Standard Acid Wash Oxalic 3-5% or HCl 3-5% Cake moisture rising >2% above baseline Every 14-30 days 60-120 min soak
Deep Regeneration HNO₃ 2-4% or HCl 5%, heated Permeability <70% of baseline after standard wash Quarterly or on-demand 2-4 hrs offline

SOP 03 -- Zero-Damage Cake Discharge

Scraper Adjustment & Zero-Damage Plate Replacement

The scraper is the component most likely to cause premature plate failure when incorrectly set. A gap that is too tight causes hard contact between the scraper blade and the ceramic membrane surface -- even a single pass can scratch through the 0.3-0.5 mm microporous membrane layer, permanently destroying filtration performance in that zone. Our plates are precision-ground to a flatness tolerance of ±0.3 mm across the full plate face, enabling reliable calibration of the scraper gap to the optimal 0.5-1.0 mm working distance.

Why ±0.3 mm flatness matters for scraper calibration

A plate with poor flatness -- surface variation of ±1.0 mm or more -- forces the maintenance team to choose between two bad options: set the scraper gap wide enough to clear the high spots (leaving cake on the low spots) or set it tight enough to clean the low spots (causing hard contact on the high spots). Our precision-ground surface eliminates this dilemma. With ±0.3 mm flatness guaranteed across the plate face, a single gap setting of 0.5-1.0 mm simultaneously ensures:

  • 100% cake discharge -- the scraper reaches every point on the plate surface within the 0.5-1.0 mm clearance window
  • Zero membrane contact -- the minimum 0.5 mm gap prevents the scraper blade from physically touching the ceramic membrane at any point
  • Consistent moisture output -- uniform cake removal prevents re-absorption of moisture from undischarged cake residue

Scraper gap calibration procedure

  1. Lock out and isolate the disc filter

    Engage full LOTO (lockout/tagout) before any scraper adjustment. Rotating disc filters can cause severe injury. Drain the slurry tank to the minimum level and confirm the drive is de-energised.

  2. Set initial gap using feeler gauge

    Using a calibrated feeler gauge, set the scraper blade-to-plate distance to 0.8 mm as the starting point (centre of the 0.5-1.0 mm target range). Check at three positions across the scraper width: drive side, centre and free end. Adjust the mounting bracket until all three readings are within ±0.1 mm of each other.

  3. Run a single-revolution dry check

    With the slurry tank drained, manually rotate the disc through one full revolution while observing the scraper-to-plate clearance. The gap should remain visually consistent. Any point where the scraper visibly contacts or deflects against the plate surface must be investigated -- check for plate warpage or scraper bracket misalignment.

  4. Verify cake discharge in first production cycle

    During the first operating cycle after adjustment, inspect the discharge chute for complete cake release. Residual cake patches adhering to the plate surface after passing the scraper indicate the gap is too wide -- reduce in 0.1 mm increments until clean discharge is achieved, but never below 0.5 mm total clearance.

  5. Check and record gap monthly

    Scraper blade wear and bracket vibration fatigue will gradually close the gap over time. Re-measure with a feeler gauge at every monthly maintenance interval and readjust as needed. Replace the scraper blade when wear reduces its thickness by more than 20% of original specification.

Technician calibrating scraper gap on ceramic disc filter using feeler gauge measurement tool

Zero-Damage Replacement Protocol

Replacing plates without membrane damage

The ceramic membrane layer is 0.3-0.5 mm thick and is the most vulnerable part of the plate during handling and installation. Follow these rules to eliminate installation-induced membrane damage:

  • Always use rubber-padded handling tools

    Never use metal hooks, bars or clamps directly against the membrane surface. Use rubber-lined lifting cradles or fabric slings.

  • Inspect plate flatness before mounting

    Lay the plate on a flat reference surface and check for rocking. Any plate with flatness deviation exceeding ±0.5 mm should be rejected -- it will cause uneven scraper contact and vacuum loss.

  • Replace friction rings and seals simultaneously

    A new plate against a worn friction ring will leak vacuum from day one. Always fit new friction rings and perimeter seals when installing replacement plates.

  • Apply torque in a cross-pattern sequence

    Tighten mounting bolts in opposing pairs (cross-pattern), not sequentially around the perimeter. This distributes clamping load evenly and prevents the plate from bowing at the centre -- which would immediately violate the ±0.3 mm flatness specification.

  • Re-calibrate scraper gap after every plate change

    Even plates of identical specification may have minor dimensional variation. Always re-measure and re-set the scraper gap after installing any replacement plate before returning the disc to service.

Plate Flatness

±0.3 mm

Precision ground tolerance

Scraper Gap

0.5-1.0 mm

Optimal working clearance

Membrane Depth

0.3-0.5 mm

Microporous layer thickness

SOP 04 -- Field Troubleshooting

Fault Diagnosis & Field Checklist

Use the following diagnostic table when performance deviates from baseline. Each symptom maps to the most probable root causes, ranked by frequency of occurrence in field operations. Start with the highest-probability cause and work down the list before escalating to plate replacement.

Field fault diagnosis checklist: symptoms, probable causes, diagnostic checks and corrective actions
Symptom Probable Root Cause Diagnostic Check Corrective Action Priority
Symptom Group A -- High Filter Cake Moisture
Cake moisture consistently 2-5% above baseline Pore blockage from fine mineral accumulation or scale deposition Run permeability flow-rate test. Compare to baseline. If <70% of original flow, pore blockage confirmed. Initiate standard acid wash (oxalic 3-5% or citric 5-8%). Repeat backwash pulse sequence at 0.15-0.20 MPa. Medium
Cake moisture elevated on specific discs only Vacuum leak on affected disc -- worn friction ring or loose water nozzle connection Apply soapy water or use ultrasonic leak detector around disc perimeter seals and nozzle fittings during vacuum draw-down. Replace friction ring and re-torque all nozzle connections on affected disc. Re-test vacuum integrity before returning to service. High
Cake moisture rising gradually over weeks Progressive scraper gap widening due to blade wear -- incomplete cake discharge leaving moisture-laden residue Measure scraper gap with feeler gauge. Compare to last recorded setting. Inspect blade for wear profile and thickness reduction. Re-calibrate scraper gap to 0.5-1.0 mm. Replace blade if wear exceeds 20% of original thickness. Medium
Uneven cake thickness across disc face Non-uniform vacuum distribution -- partially blocked internal filtrate channel or cracked plate sector Remove disc from service. Perform individual sector vacuum test. Inspect internal filtrate channel for scale or debris blockage. Flush filtrate channel with high-pressure water. Replace any cracked or non-sealing plate sectors. High
Symptom Group B -- Insufficient Vacuum / Vacuum Loss
System vacuum below target across all discs Vacuum pump capacity loss -- wear ring clearance increase, liquid ring water temperature too high, or inlet filter blocked Measure pump inlet vacuum with calibrated gauge. Check liquid ring water temperature (should be <30 °C). Inspect pump inlet screen. Service or replace pump wear rings. Reduce liquid ring water temperature. Clean inlet filter screen. High
Vacuum drops rapidly during cake formation phase Friction ring air leak on one or more discs allowing atmospheric air ingress into the vacuum manifold Isolate discs one at a time from the vacuum manifold. Identify which disc causes the largest vacuum recovery when isolated. Replace friction ring on identified disc. Inspect all disc-to-shaft interface seals. Verify torque on all mounting hardware. High
Vacuum normal but cake forms slowly Pore blockage reducing effective filtration area -- backwash frequency insufficient for current slurry solids loading Check backwash discharge clarity. Measure permeability flow rate on representative plates. Compare to baseline. Increase backwash frequency to every 4 hours. Initiate acid wash cycle. Review backwash pressure -- confirm 0.15-0.20 MPa at manifold. Medium
Intermittent vacuum fluctuation during rotation Loose or worn water nozzle (filtrate outlet fitting) on one or more plate sectors -- intermittent air ingress as nozzle passes the vacuum valve Observe vacuum gauge during rotation. Note rotational position at which vacuum drops. Identify corresponding sector and inspect nozzle fitting. Re-torque or replace water nozzle fittings on identified sectors. Apply thread sealant if nozzle threads show wear. Medium
Symptom Group C -- Turbid or Contaminated Filtrate
Filtrate suddenly becomes turbid -- all discs affected Through-crack in one or more plates allowing slurry bypass directly into the filtrate stream Remove all discs from service. Perform individual plate pressure test (apply 0.05 MPa air to filtrate port; observe bubble formation on membrane face under water). Replace all plates that show air passage through the membrane body. Do not return cracked plates to service -- slurry bypass will contaminate the entire filtrate circuit. Critical
Filtrate turbidity limited to one disc position Localised membrane damage -- scraper hard contact, impact damage or edge chip propagated to through-crack Isolate suspect disc from filtrate manifold. Confirm turbidity disappears. Inspect all plates on that disc for visible membrane damage. Replace damaged plate(s). Re-calibrate scraper gap to prevent recurrence. Investigate impact event if no scraper contact is evident. Critical
Gradual increase in filtrate suspended solids over days Micropore enlargement from abrasive wear or chemical over-etching -- membrane pore size drifting above rated specification Measure filtrate turbidity (NTU). Compare to baseline. Inspect plate surface under magnification for pore enlargement or surface erosion patterns. Review acid wash concentration history -- reduce if over-etching suspected. Schedule plate replacement for affected discs. Adjust feed solids concentration if abrasion is the driver. Medium
Filtrate turbid only during backwash cycle Normal -- fine mineral fines flushed from pores during backwash appear in filtrate momentarily. Only a concern if it persists beyond 30 seconds post-backwash. Time the duration of post-backwash turbidity. If clarity returns within 30 seconds, no action needed. If turbidity persists, check for plate cracking. If turbidity resolves within 30 sec: no action required. If persistent: follow cracked plate diagnosis protocol above. Low

Priority Level

Low

Monitor and address at next scheduled maintenance window. No immediate production impact.

Priority Level

Medium

Address within 24-48 hours. Performance degrading; continued operation without correction will accelerate plate wear.

Priority Level

High / Critical

Stop affected disc or full machine immediately. Continued operation risks cascading damage or filtrate contamination of downstream processes.

Maximising plate service life

Achieving 13+ months of plate service life

Service life of 13 months or longer is achievable in the majority of mineral processing applications when the four maintenance disciplines described in this guide are applied consistently. The following factors determine whether your operation reaches this target.

Backwash discipline (highest impact)

Operations that maintain 8-hourly pulse backwash at 0.15-0.20 MPa consistently report 40-60% longer plate life than those running daily or lower-frequency backwash. Pore blockage is cumulative and accelerating -- early prevention is far more effective than late-stage remediation.

Timely chemical cleaning

Scale that is allowed to mineralise over weeks becomes increasingly difficult to remove without aggressive acid concentrations. Weekly light acid washes prevent scale from hardening into permanent pore obstruction. Our pH 1-14 resistant ceramic enables these frequent cleaning cycles without degradation risk.

Correct scraper gap maintenance

Scraper hard contact is the single largest cause of premature membrane failure in field operations. Monthly gap verification at the 0.5-1.0 mm specification, combined with timely blade replacement, eliminates this failure mode entirely.

Structured wear assessment

Quarterly permeability testing identifies plates approaching end-of-life before they fail in service. Planned replacement is 3-5× less costly than emergency replacement -- and prevents the cascade damage that one failed plate can cause to adjacent plates and friction rings.

Typical plate service life by application & maintenance level

Ore Type Poor Maintenance This SOP Applied
Iron ore (concentrate) 6-9 months 13-18 months
Iron ore (tailings) 8-12 months 15-22 months
Copper concentrate 5-8 months 13-16 months
Gold / silver 8-14 months 16-24 months
Lithium (spodumene) 7-10 months 13-18 months
Nickel / lead-zinc 6-10 months 13-20 months

Estimates based on field data from operations using our monolithic sintered plates. Actual life depends on feed abrasiveness, solids loading and operating hours per day.

Common field questions

Maintenance engineering FAQ

Can I run backwash at higher than 0.20 MPa to clean more aggressively?
We do not recommend exceeding 0.20 MPa for routine backwash. While our monolithic plates are structurally rated to withstand higher pressures, repeated cycles above 0.20 MPa create micro-fatigue stress at the pore throat walls over time, gradually enlarging pore diameter and ultimately reducing filtration selectivity. The 0.15-0.20 MPa range is optimised to provide maximum fine-particle ejection force without progressive pore enlargement. For severely blocked plates that do not respond to standard backwash, escalate to chemical cleaning rather than increasing pressure.
How do I know when to replace versus clean a blocked plate?
Replace rather than clean when: (1) permeability flow rate remains below 50% of original baseline after a full deep-clean cycle including acid wash, (2) any through-crack or delamination is detected during visual or pressure inspection, (3) edge chipping exceeds 5 mm depth at more than two locations, or (4) the plate membrane shows visible surface erosion or pore enlargement under magnification. Cleaning restores blocked-but-intact pores; it cannot repair structural damage or reverse abrasive membrane wear.
Is it safe to use alkaline cleaning solutions on our ceramic plates?
Yes. Our integral-sintered alumina ceramic is chemically stable across the full pH 1-14 range. Dilute sodium hydroxide (NaOH at 2-4% concentration, pH 12-13) or sodium carbonate solutions are effective for removing organic residues, flotation reagent films and certain silicate deposits that acid washing does not dissolve. Alkaline cleaning is particularly useful in gold processing circuits where cyanide-related organic residues accumulate on plate surfaces. Always rinse thoroughly with clean water after alkaline cleaning and verify pH returns to 6-8 before returning plates to service.
What scraper blade material is compatible with ceramic filter plates?
Polyurethane (PU) and ultra-high-molecular-weight polyethylene (UHMWPE) are the recommended scraper blade materials for ceramic filter plates. Both are softer than the alumina ceramic membrane surface -- if the gap setting drifts and the blade makes contact, the blade deforms rather than scratching the ceramic. Never use metal or hardened steel scraper blades against ceramic plates; even a brief contact event at operating speed will score the membrane surface and create a filtrate bypass channel. Rubber blades are acceptable for low-abrasion applications but wear faster than PU in high-solids slurry environments.
How do I confirm the 13+ month lifespan target is being achieved at my site?
Track three leading indicators on a monthly basis: (1) permeability retention -- measure flow rate on 10% of plates each month and track the trend against the baseline; plates maintaining >80% of original flow rate at 12 months are on track for 13+ month life; (2) cake moisture trend -- log average cake moisture per shift; a stable or improving trend confirms plate and scraper condition are being maintained; (3) backwash pulse count to clarity -- log how many pulses are needed to achieve discharge clarity each session; a stable count confirms scale is not accumulating. Contact our technical team to receive a free monthly tracking spreadsheet template for these three metrics.

Request a service assessment

Talk to a maintenance engineering specialist

Tell us your machine model, current plate condition and maintenance challenges. Our engineers will recommend a backwash program, chemical cleaning protocol and spare-parts package tailored to your ore type and operating conditions.

  • On-site or remote assessment

    We support both in-person site visits and remote assessment via photos, data sheets and video inspection.

  • Rapid response

    Initial technical response within 24 hours. Emergency spare-parts quotation within 48 hours for critical breakdowns.

  • All filter platforms, all minerals

    Service protocols for all major vacuum ceramic disc filter platforms across iron ore, copper, gold, lithium, nickel and lead-zinc operations.

Technical drawings, photos and maintenance logs can be sent by email after initial contact. We respond within 24 hours.